PVD COATING FOR TOOLS AND WORKPIECES
Part of our reconditioning service is PVD coating. A PVD coating on a resharpened tool restores its initial performance and extends the life cycle. Recoating is necessary to preserve cutting parameters and useful life set for production lines. It also helps increase edge durability, smoothens chip evacuation, and reduces friction and heat. Part of our reconditioning service is PVD coating. A PVD coat on a resharpened tool restores its initial performance and extends the life cycle. Recoating is necessary to preserve cutting parameters and useful life set for production lines. It also helps increase edge durability, smoothens chip evacuation, and reduces friction and heat.
Shell | ShellGrubość [μm] | Micro hardness** | Coefficient of friction* | Operating(°C) |
TiN | 2 - 4 | 2300 - 2800 | 0.4 - 0.5 | 600 |
TiAlN | 2 - 4 | 3200 - 3300 | 0.3 - 0.6 | 900 |
AlTiN | 2 - 4 | 3300 - 3500 | 0.4 - 0.6 | 900 |
TiCN | 1 - 3 | 2800 - 3000 | 0.2 - 0.4 | 400 |
TiN Coating – universal
Recommended use:
TiAlN coating – increases the thermal and chemical resistance and stability of cutting edges
Recommended use:
AlTiN coating – suitable for high performance cutting (HSC, HPC) and machining hard materials.
Recommended use:
TiCN coating – with a low coefficient of friction and hardness. It allows you to work in temperatures up to 400°C.
Recommended use: